Needle Penetration Force Test for Hypodermic and Pen Needles

By Lim Xu, Export Manager

A needle penetration force test records the force as a hypodermic or pen needle pierces a specified test film or membrane. The curve is used to judge tip sharpness and the drag of the needle body, not the penetration of asphalt or wax.

What penetration force says about needle sharpness

A sharp, well-finished tip usually needs less force to start the puncture, and the force then settles into a lower drag as the tube follows. A dull, hooked or damaged tip raises the first peak and can tear the film.

The test is a laboratory comparison, not a clinical pain score. It is used to check incoming needles, to compare lots, and to see whether a grind or a coating change has moved the force curve.

Named methods for this kind of work include ISO 7864 for sterile hypodermic needles, DIN 13097-4, ISO 9626 for needle tubing, and ISO 11608-2 for needles used with pen systems. This article does not claim that each of those texts sets the same film or speed. Check the method you follow, and please confirm with us before you treat an instrument setup as matching a named standard.

Test film, speed and fixture

The film, the clamp and the test speed all change the curve. A thicker or tougher film raises the peak. A different speed changes how the tip and the film interact. A loose clamp lets the film stretch and rounds the peak.

Take the film, the speed and the fixture from the method text. Until those details are confirmed against the standard you use, this article does not quote them.

The needle has to be held on its hub or shaft so that it meets the film squarely. A tilted needle, a bent tube or a fixture that lets the tip skate will raise the force and spoil the comparison.

Our needle puncture force tester is the instrument we offer for this work. Whether a given load cell, speed and fixture match the method you follow is something to confirm with us first.

Questions about a model or a test? Email Amy Zhao, Export Manager, at [email protected].

Reading the force curve

The useful record is the force-displacement curve, not a single number taken at random on the rise. Most reports pick a peak at the moment the tip breaks through, then a drag value as the tube travels through the film.

Tip penetration peak

The first peak is the force needed to start the puncture. Compare it with the limit in your specification, and with the curve from a retained lot you already trust.

A second bump just after the peak can mean the bevel has caught, or the film has torn unevenly. Photograph the tip if a lot starts to show that shape.

Drag force

After the tip is through, the force often falls and then holds as the shaft slides through the hole. That held value is the drag, and it is sensitive to diameter, finish and coating.

A rising drag through the stroke can mean a rough tube, a damaged coating or a film that is closing on the shaft. Report both the peak and the drag, and say over which part of the stroke the drag was read.

Penetration force vs stopper puncture force

A needle penetration force test uses a specified film to judge the needle. A stopper puncture test pushes the needle through an elastomeric closure, such as a vial stopper, and records that force.

The two tests answer different questions. Film penetration is about the needle. Stopper puncture is about the needle and the closure together, and the stopper formulation, lubrication and thickness all matter.

If you are checking needles, use the film method in the needle standard you follow. If you are checking a closure system, use the stopper method named for that system, and do not treat the two peaks as the same specification.

A finished pack still needs its own integrity check. A blister leak test is one example, and it does not replace a needle penetration force test.

Sampling and reporting

Needles vary along a lot, so a single needle is not a result. Take a sample plan from the specification or from your quality procedure, and keep the unused needles in their packaging until the test.

Report the method, the film, the speed, the peak force, the drag, the needle gauge or nominal size, and any pretreatment such as a lubricant check. If the tester stores curves, keep the curve with the report, because a later dispute is hard to settle from a peak alone.

Do not average peaks from two different films or speeds. If a method or a customer changes the film, start a new baseline.

Frequently asked questions

Does this test apply to asphalt needle penetration?

No. Asphalt or bitumen needle penetration is a different method, used on paving materials. This article covers hypodermic and pen needles only.

Does a lower peak always mean a better needle?

Not by itself. A very low peak with a torn film, a bent tube or a skipped bevel can be a fault. Read the whole curve and inspect the tip.

What should I send with a request for a quotation?

Tell us the needle type, the method you follow, and whether you also need stopper puncture. We can then say which setup to consider and send you a quotation.

Talk to our factory team

We sell direct from our factory, so you work directly with our factory team. Questions about a model or a test? Email Amy Zhao, Export Manager, at [email protected].

Related articles

Let's Talk

We're here to help you with your needs. Let's talk about how we can help you.

View our privacy policy.

© 2026 KHT Instruments | All rights reserved.